1101/1102 lmitation Dyeing

Product Introduction

Good air permeability, no hand feel, soft, easy to operate, suitable for rotary screen and flat screen printing.


1. Product Description
1.1 Category:Imitated discharge paste
1.2 Features:Excellent breathability,zero glue feel
1.3 Applicable fabrics:Suitable for light-colored fabrics
1.4 Storage:Keep sealed and store in a cool and ventilated place between 5-40℃ of temperature
1.5 Eco-friendly:Compliant with OEKO-TEX and other relevant standards

2. Application Ratio

Note:
1.It is recommended to use the high temperature migration resistant color paste.
2.The total amount of color paste is recommended not to exceed 10%, otherwise it w ill fade or migrate.

3. Printing Process
3.1 Printing condition
A. It is recommended to operate under 40% to 70%humidity conditions,and pay attention to the effect of temperature on operability.When the humiditshuy is higher than 70%,the heating time shall be appropriately extended to avoid the surface becoming sticky and the washing fastness becoming poor;when the humidity is lower than 40%,1-3% moisturizer shall be added to prevent the screen from blocking.
B. Squeegee:55-65 hardness oily squeegee
C. Mesh:100-120 mesh
D. Curing conditions:130-135℃ for 2 minutes

4.Performance Of Printed Products

Test Project11011102Test Method
FlexibilityLevel 4Level 4Internal standard:Level5 very sof
ElasticityInternal standard:Level5 very sof
WhitenessLevel 3Internal standard:Level5 very best
Covering propertyLevel 3Internal standard:Level5 very best
Machine wash fastnessPassPass40℃Water temperature,20g of phosphate free laundry detergent,1000 rpm,standard wash for 90 minutes*5 times
Resistant to dry rubbing color fastnessLevel 3Friction for 20 cycles
Moisture resistant rubbing color fastnessLevel 3Friction for 20 cycles
Freeze resistanceStandard temperature -25℃,frozen for 24 hours

Note:The product performance and application data listed above were obtained under specific experimental conditions,and the actual usage environment of the product is variable.Customers need to undergo testing before mass production.For any unclear information,please contact Guangdong Caigle Technology Co.,Ltd.We reserve the right to revise the product manual without further notice.

5.Frequently Asked Questions

ProblemPossible CauseSolution
Glue sensitivityExcessive printing timesPrint1-2 times,recommend to print once
Poor Adhesion1.Insufficient cross-linking time
2.Insufficient overheating temperature and time
1. Let it stand for 8-12 hours
2.Overheating at 130-135℃ for 2minutes
Screen Plugging1.The paste is too thick
2.The humidity is too low
Add moisturizing agents with proportion not exceeding 3%
Scroll to Top