216 Windcoat Under BasePaste

Product Introduction

It has strong adhesion, good fastness, scratch resistance, soft hand feel, does not scratch cloth, and can widely replace traditional base ink.


1.Product Description
1.1 Category:Windcoat under base paste
1.2 Features:Soft hand feel,excellent film-forming property,strong adhesion, good fastness and scratch resistance
1.3 Applicable fabrics:Suitable for swimsuit fabric,windbreaker fabric,umbrella fabric,nylon fabric,polyester fabric,etc
1.4 Storage:Keep sealed and store in a cool and ventilated place between 5-40℃ of temperature
1.5 Eco-friendly:Compliant with OEKO-TEX and other relevant standards

2.ApplicationRatio
Add 2% PC200 additives

3.Printing Process
3.1 Printing condition
A. It is recommended to operate under 40% to 70%humidity conditions,and pay attention to the effect of temperature on operability.When the humiditshuy is higher than 70%,the heating time shall be appropriately extended to avoid the surface becoming sticky and the washing fastness becoming poor;when the humidity is lower than 40%,1-3%moisturizer shall be added to prevent the screen from blocking.
B. Squeegee:55-65 hardness oily squeegee
C. Mesh:100-120 mesh
D. Curing conditions:130-135℃ for 2 minutes

4. Performance Of Printed Products

Test Project216Test Method
FlexibilityLevel 4Internal standard: Level 5 very soft
ElasticityLevel 5Internal standard: Level 5 very soft
Machine wash fastnessPass40℃Water temperature,20g of phosphate free laundry detergent,1000 rpm,standard wash for 90 minutes*5 times

Note:The product performance and application data listed above were obtained under specific experimental conditions,and the actual usage environment of the product is variable.Customers need to undergo testing before mass production.For any unclear information,please contact Guangdong Caigle Technology Co.,Ltd.We reserve the right to revise the product manual without further notice.

5. Frequently Asked Questions

ProblemPossible CauseSolution
Printing Poor Crack1.Insufficient cross-linking time
2.The paste is not dry ,causing tearing due to peeling
1.Add additives in proportion
2.Operate according to the printing process
Poor Adhesion1.Insufficient cross-linking time
2.Insufficient overheating temperature and time
1.Let it stand for 8-12 hours
2.Overheating at 130-135℃ for 2minutes
Screen Plugging1.The slurry is too thick
2.The humidity is too low
Add moisturizer agents with proportion not exceeding 3%
Scroll to Top