302 Anti-freezing Nylon Thick Plate Slurry

Product Introduction

Strong three-dimensional effect and good washing fastness Good transparency and anti- freezing at-25°C.


1.Product Description
1.1 Category:Machine printing high density paste
1.2 Feature:Excellent fastness,soft hand feel,and non-sticky surface)
1.3 Applicable fabrics:Suitable for all types of fabrics
1.4 Storage:Keep sealed and store in a cool and ventilated place between 5-40℃ of temperature
1.5 Eco-friendly:Compliant with OEKO-TEX and other relevant standards

2.Application Ratio
Ready for immediate use

3.Printing Process
3.1 Printing condition
A. It is recommended to operate under 40% to 70%humidity conditions,and pay attention to the effect of temperature on operability.When the humiditshuy is higher than 70%,the heating time shall be appropriately extended to avoid the surface becoming sticky and the washing fastness becoming poor;when the humidity is lower than 40%,1-3%moisturizer shall be added to prevent the screen from blocking.
B. Squeegee:55-65 hardness oily squeegee
C. Mesh:100-120 mesh
D. Curing conditions:130-135℃ for 2 minutes

4. Performance Of Printed Products

Test Project302Test Method
FlexibilityLevel 3Internal standard: Level 5 very soft
Machine wash fastnessPass40℃Water temperature,20g of phosphate free laundry detergent,1000 rpm,standard wash for 90 minutes*5 times

Note:The product performance and application data listed above were obtained under specific experimental conditions,and the actual usage environment of the product is variable.Customers need to undergo testing before mass production.For any unclear information,please contact Guangdong Caigle Technology Co.,Ltd.We reserve the right to revise the product manual without further notice.

5. Frequently Asked Questions

ProblemPossible CauseSolution
PrintingPoor Crack1.Insufficient cross-linking time
2.The paste is not dry ,causing tearing due to peeling
1.Add additives in proportion
2. Operate accordance to the printing process
Poor Adhesion1. Insufficient cross-linking time
2. Insufficient overheating temperature and time
1.Let it stand for 8-12 hours
2.Overheating at 130-135℃ for 2minutes
Screen Plugging1.The paste is too thick
2.The humidity is too. low
Add moisturizer agents with proportion not exceeding 3%
Scroll to Top