1.Product Description
1.1 Category:Special effect paste
1.2 Features:Good sublimation prevention effect
1.3 Applicable fabrics:Suitable for cotton fabric,knitted fabric,etc
1.4 Storage:Keep sealed and store in a cool and ventilated place between 5-40℃ of temperature
1.5 Eco-friendly:Compliant with OEKO-TEX and other relevant standards
2.Application Ratio
| Product name | Ratio % |
|---|---|
| 501 | 70-90 |
| Clear paste | 10-30 |
3.Printing Process
3.1 Printing condition
A. Itis recommended to operate under 40% to 70%humidity conditions,and pay attention to the effect of temperature on operability.When the humiditshuy is higher than 70%,the heating time shall be appropriately extended to avoid the surface becoming sticky and the washing fastness becoming poor;when the humidity is lower than 40%,1-3%moisturizer shall be added to prevent the screen from blocking.
B. Squeegee:55-65 hardness oily squeegee
C. Mesh:100-120 mesh
D. Curing conditions:130-135℃ for 2 minutes
4.Performance Of Printed Products
| Test Project | 501 | Test Method |
|---|---|---|
| Flexibility | Level 3 | Internal standard:Level5 very soft |
| Elasticity | —— | Internal standard:Level 5 very soft |
| Whiteness | —— | Internal standard:Level5 the best |
| Covering property | Level 4 | Internal standard:Level5 the best |
| Machine wash fastness | Pass | 40℃Water temperature,20g of phosphate free laundry detergent,1000 rpm,standard wash for 90 minutes*5 times |
| Resistant to dry rubbing color fastness | —— | Friction for 20 cycles |
| Moisture resistant rubbing color fastness | —— | Friction for 20 cycles |
| Freeze resistance | —— | Standard temperature -25℃,frozen for 24 hours |
Note:The product performance and application data listed above were obtained under specific experimental conditions,and the actual usage environment of the product is variable.Customers need to undergo testing before mass production.For any unclear information,please contact Guangdong Caigle Technology Co.,Ltd.We reserve the right to revise the product manual without further notice.
5.Frequently Asked Questions
| Problem | Possible Cause | Solution |
|---|---|---|
| Poor anti-sublimation effect | 1.Anti sublimation paste printing times less, the thickness is not enough 2.Too much transparent paste ratio, resulting in less sublimation paste ratio 3.The sublimation of the fabric is serious | 1.Increase the number of anti-sublimation paste prints 2.Prepare according to the application ratio 3.Change the cloth or change the sublimation paste |
| Paste Poor Crack | 1.Insufficient cross-linking time 2.The paste is not dry ,causing tearing due to peeling | 1.Add additives in proportion 2.Operate according to the printing process |
| Poor Adhesion | 1.Insufficient cross-linking time 2.Insufficient overheating temperature and time 3.Anti-sublimation paste is not used with clear paste | 1.Let it stand for 8-12 hours 2.Overheating at 130-135℃ for 2minutes 3.Prepare according to the application ratio |
| Screen Plugging | 1.The slurry is too thick 2.The humidity is too low | Add moisturizing agents with proportion not exceeding 3% |