531/532 Nylon Dot Paste

Product Introduction

It is scratch-resistant, wear.resistant, and has good durability. It meets the reguirements of machine washing, acid and alkali resistance, water cracking during washing, soft hand feel, and good elasticity.


1. Product Description
1.1 Category:Nylon high mesh white/clear paste
1.2 Features:soft hand feel,good color development,good washing fastness, good mesh passing performance
1.3 Applicable fabrics:Polyester fabric,nylon fabric,swimsuit fabric,etc
1.4 Storage:Keep sealed and store in a cool and ventilated place between 5-40℃ of temperature
1.5 Eco-friendly:Compliant with OEKO-TEX and other relevant standards

2. Application Ratio

Note:
1.It is recommended to use the high temperature migration resistant color paste.
2.The total amount of color paste is recommended not to exceed 10%, otherwise it w ill fade or migrate.
3.Add 2% PC200 additives.

3. Printing Process
3.1 Printing condition
A. It is recommended to operate under 40% to 70%humidity conditions,and pay attention to the effect of temperature on operability.When the humiditshuy is higher than 70%,the heating time shall be appropriately extended to avoid the surface becoming sticky and the washing fastness becoming poor;when the humidity is lower than 40%,1-3% moisturizer shall be added to prevent the screen from blocking.
B. Squeegee:55-65 hardness oily squeegee
C. Mesh:135-150 mesh
D. Curing conditions:130-135℃ for 2 minutes,or natural drying for 2-3 days.

4.Performance Of Printed Products

Test Project531532Test Method
FlexibilityLevel 3Level 3Internal standard:Level5 very sof
WhitenessLevel 3Internal standard:Level5 very best
Covering propertyLevel 3Internal standard:Level5 very best
Machine wash fastnessPassPass40℃Water temperature,20g of phosphate free laundry detergent,1000 rpm,standard wash for 90 minutes*5 times
Resistant to dry rubbing color fastnessLevel 4Friction for 20 cycles
Moisture resistant rubbing color fastnessLevel 4Friction for 20 cycles

Note:The product performance and application data listed above were obtained under specific experimental conditions,and the actual usage environment of the product is variable.Customers need to undergo testing before mass production.For any unclear information,please contact Guangdong Caigle Technology Co.,Ltd.We reserve the right to revise the product manual without further notice.

5.Frequently Asked Questions

ProblemPossible CauseSolution
Poor Adhesion1.Insufficient cross-linking time1. Let it stand for 8-12 hours
2.Insufficient overheating temperature and time2.Overheating at 130-135℃ for 2minutes
Screen Plugging1.The slurry is too thick or the humidity is too low
2.Line count too high
1.Add moisturizing agents with proportion not exceeding 3%
2.Reduce the line count
Scroll to Top