703/704 Elastic matte paste

Product Introduction

It has good covering power, soft hand feel and good washing fastness.


1. Product Description
1.1 Category:Machine-printing white/clear paste
1.2 Features:Good coverage,dry and comfortable to the touch
1.3 Applicable fabrics:Suitable for cotton,knitted fabrics,etc
1.4 Storage:Keep sealed and store in a cool and ventilated place between 5-40℃ of temperature
1.5 Eco-friendly:Compliant with OEKO-TEX and other relevant standards

2. Application Ratio

Note:
1.It is recommended to use the high temperature migration resistant color paste.
2.The total amount of color paste is recommended not to exceed 10%, otherwise it w ill fade or migrate.

3. Printing Process
3.1 Printing condition
A. It is recommended to operate under 40% to 70%humidity conditions,and pay attention to the effect of temperature on operability.When the humiditshuy is higher than 70%,the heating time shall be appropriately extended to avoid the surface becoming sticky and the washing fastness becoming poor;when the humidity is lower than 40%,1-3% moisturizer shall be added to prevent the screen from blocking.
B. Squeegee:55-65 hardness oily squeegee
C. Mesh:100-120 mesh
D. Curing conditions:130-135℃ for 2 minutes,or natural drying for 2-3 days

4.Performance Of Printed Products

Test Project703704Test Method
FlexibilityLevel 4Level 4Internal standard:Level5 very sof
ElasticityInternal standard:Level5 very sof
WhitenessLevel 3-4Internal standard:Level5 very best
Covering propertyLevel 3-4Internal standard:Level5 very best
Machine wash fastnessPassPass40℃Water temperature,20g of phosphate free laundry detergent,1000 rpm,standard wash for 90 minutes*5 times
Resistant to dry rubbing color fastnessLevel 3Friction for 20 cycles
Moisture resistant rubbing color fastnessLevel 3Friction for 20 cycles
Freeze resistancePassStandard temperature -25℃,frozen for 24 hours

Note:The product performance and application data listed above were obtained under specific experimental conditions,and the actual usage environment of the product is variable.Customers need to undergo testing before mass production.For any unclear information,please contact Guangdong Caigle Technology Co.,Ltd.We reserve the right to revise the product manual without further notice.

5.Frequently Asked Questions

ProblemPossible CauseSolution
Paste Poor Crack1.Insufficient cross-linking time
2.The paste is not dry ,causing tearing due to peeling
1.Add additives in proportion
2.Operate according to the printing process
Poor Adhesion1.Insufficient cross-linking time
2.Insufficient overheating temperature and time
1.Let it stand for 8-12 hours
2.Overheating at 130-135℃ for 2minutes
Screen Plugging1.The paste is too thick
2.The humidity too low
Add moisturizing agents with proportion not exceeding 3%