809 Skin-Feel Matte

Product Introduction

It has a soft, fine and smooth touch,  leaves no trace when touched,and has excellent skin-friendliness.It has a strong matte finish, good transparency, and does not tum white when pulled apart . The dry and wet wiping grades can reach 4-5 levels.


1.Product Description
1.1 Category:Skin-feel top coating paste
1.2 Features:Good matte effect,good transparency,soft hand feel,dry-wet rubbing is over grade 4.5
1.3 Applicable fabrics:All fabrics
1.4 Storage:Keep sealed and store in a cool and ventilated place between 5-40℃ of temperature
1.5 Eco-friendly:Compliant with OEKO-TEX and other relevant standards

2.Application Ratio
2.1 It needs to add 1%PC200 additives when use this product.
2.2 Ensure the printing surface is dry and not wet before printing the covering paste.

3.Printing Process
3.1 Printing condition
A. It is recommended to operate under 40% to 70%humidity conditions,and pay attention to the effect of temperature on operability.When the humiditshuy is higher than 70%,the heating time shall be appropriately extended to avoid the surface becoming sticky and the washing fastness becoming poor;when the humidity is lower than 40%,1-3%moisturizer shall be added to prevent the screen from blocking.
B. Squeegee:55-65 hardness oily squeegee
C. Mesh:100-120 mesh
D. Overheating condition: 130–135°C for 2 minutes

4.Performance Of Printed Products

Test Project809Test method
FlexibilityLevel 5Internal standard: Level 5 very soft
Machine wash fastnessPass40℃ Water temperature,20g of phosphate free laundry detergent,1000 rpm,standard wash for 90 minutes*5 times
Resistant to dry rubbing color fastness4–5 gradeFriction for 20 cycles
Moisture resistant rubbing color fastness4–5 gradeFriction for 20 cycles
Freeze resistancePassStandard temperature -25℃,frozen for 24 hours

Note appended:The product performance and application data listed above were obtained under specific experimental conditions,and the actual usage environment of the product is variable.Customers need to undergo testing before mass production.For any unclear information,please contact Guangdong Caigle Technology Co.,Ltd.We reserve the right to revise the product manual without further notice.

5.Frequently Asked Questions

ProblemPossible causeSolution
Paste Poor Crack1.Insufficient cross-linking time
2. The paste is not dry ,causing tearing due to peeling
1. Add additives in proportion
2.Operate according to the printing process
Poor Adhesion1. Insufficientcross-linking time
2.Insufficient overheating temperature and time
1.Let it stand for 8-12 hours
2.Overheating at 120-135℃ for 2minutes
Screen Plugging1.The slurry is too thick
2.The humidity is too low
Add moisturizing agents with proportion not exceeding 3%