1. Product Description
1.1 Category:Binder
1.2 Features:Soft hand feel,Good dry and wet rubbing fastness and bright color
1.3 Applicable fabrics:Suitable for Suitable for cotton,knitted fabrics,etc
1.4 Storage:Keep sealed and store in a cool and ventilated place between 5-40℃ of temperature
1.5 Eco-friendly:Compliant with OEKO-TEX and other relevant standards
2.ApplicationRatio
| Product | Addition amount % |
| A002 | 5-25 |
| Water | 75-95 |
Note:
1、Add less than 6% color paste, thicken viscosity with 799 thickener to 30,000-50,000 mpas
2、For dark-colored printed fabrics, it is recommended to add 2% 839 fixer to enhance the fastness to water washing and dry and wet rubbing. Stir thoroughly before use.
3.Printing Process
3.1 Printing condition
A. It is recommended to operate under 40% to 70%humidity conditions,and pay attention to the effect of temperature on operability.When the humiditshuy is higher than 70%,the heating time shall be appropriately extended to avoid the surface becoming sticky and the washing fastness becoming poor;when the humidity is lower than 40%,1-3%moisturizer shall be added to prevent the screen from blocking.
B. Squeegee:55-65 hardness oily squeegee
C. Mesh:100-120 mesh
D. Curing conditions:150-160℃ for 2 minutes
4.Performance Of Printed Products
| Test Project | A002 | Test Method |
| Flexibility | Level 5 | Internal standard:Level5 very soft |
| Elasticity | — | Internal standard:Level5 very soft |
| Whiteness | — | Internal standard:Level5 the best |
| Covering property | — | Internal standard:Level5 the best |
| Machine wash fastness | Pass | 40℃Water temperature,20g of phosphate free laundry detergent,1000 rpm,standard wash for 90 minutes*5 times |
| Resistant to dry rubbing color fastness | Level 4 | Friction for 10 cycles |
| Moisture resistant rubbing color fastness | Level 2-3 | Friction for 10 cycles |
Note:The product performance and application data listed above were obtained under specific experimental conditions,and the actual usage environment of the product is variable.Customers need to undergo testing before mass production.For any unclear information,please contact Guangdong Caigle Technology Co.,Ltd.We reserve the right to revise the product manual without further notice.
5.FrequentlyAskedQuestions
| Problem | Possible Cause | Solution |
| Poor Adhesion | 1.Insufficient cross-linking time 2.Insufficient overheating temperature and time | 1. Let it stand for 8-12 hours 2.Overheating at 150-160℃ for 2minutes |
| Screen Plugging | 1.The slurry is too thick 2.The humidity is too low | Add moisturizing agents with proportion not exceeding 3% |