309 Flocking Slurry

Product Introduction

It has a suede effect, good fastness and a softhand feel.


1.Product Description
1.1 Category:Electrostatic flocking paste
1.2 Features:Application for Suede effect, good fastness, soft feel
1.3 Applicable fabrics:Suitable for cotton fabric, polyester fabric, cotton-polyester blend,etc
1.4 Storage:Keep sealed and store in a cool and ventilated place between 5-40℃ of temperature
1.5 Eco-friendly:Compliant with OEKO-TEX and other relevant standards

2.Application Ratio
2.1 It needs to add 1% PC200 additives when use this product.

3.Printing Process
3.1 Printing condition
A. It is recommended to operate under 40% to 70%humidity conditions,and pay attention to the effect of temperature on operability.When the humiditshuy is higher than 70%,the heating time shall be appropriately extended to avoid the surface becoming sticky and the washing fastness becoming poor;when the humidity is lower than 40%,1-3%moisturizer shall be added to prevent the screen from blocking.
B. (Squeegee:55-65 hardness oily squeegee
C. Mesh:100-120 mesh
D. Curing conditions:130-135℃ for 2 minutes

4.Performance Of Printed Products

Test Project309Test Method
FlexibilityLevel 4Internal standard:Level5 very soft
Machine wash fastnessPass40℃Water temperature,20g of phosphate free laundry detergent,1000 rpm,standard wash for 90 minutes*5 times

Note :The product performance and application data listed above were obtained under specific experimental conditions,and the actual usage environment of the product is variable.Customers need to undergo testing before mass production.For any unclear information,please contact Guangdong Caigle Technology Co.,Ltd.We reserve the right to revise the product manual without further notice.

5.Frequently Asked Questions

ProblemPossible CauseSolution
Poor tomentum fastness1.The paste has surface dried before flocking1.Flocking immediately after the last paste printing
2.Insufficient overheating temperature and time2.Overheating at 130-135℃ for 2 minutes
3.The thickness of the paste is insufficient3.Increase the number of prints
4.Flocking equipment parameters are not suitable4.Re-adjust the flocking equipment parameters
Tomentum decolorizationCotton tomentum was usedSwitch to polyester tomentum