30F Gold And Silver Powder Paste

Product Introduction

It has a soft touch and good washing fastness, and is suitable for reflective powder, gold and silver powder, pearlescent powder, etc.


1. Product Description
1.1 Category:Special effects paste
1.2 Feature:Oxidation resistance,excellent fastness,soft hand feel,and non-sticky surface
1.3 Applicable fabrics:Suitable for all types of fabrics
1.4 Storage:Keep sealed and store in a cool and ventilated place between 5-40℃ of temperature
1.5 Eco-friendly:Compliant with OEKO-TEX and other relevant standards

2. ApplicationRatio

3. Printing Process
3.1 Printing condition
A. It is recommended to operate under 40% to 70%humidity conditions,and pay attention to the effect of temperature on operability.When the humiditshuy is higher than 70%,the
heating time shall be appropriately extended to avoid the surface becoming sticky and the washing fastness becoming poor;when the humidity is lower than 40%,1-3%moisturizer shall be added to
prevent the screen from blocking.
B. Squeegee:55-65 hardness oily squeegee
C. Mesh:80-100 mesh
D. Curing conditions:130-135℃ for 2 minutes

4.Performance Of Printed Products

Test Project30FTest Method
FlexibilityLevel 4Internal standard:Level5 very soft
ElasticityLevel 3Internal standard:Level5 very soft
Machine wash fastnessPass40℃Water temperature,20g of phosphate free laundry detergent,1000 rpm,standard wash for 90 minutes*5 times
Resistant to dry rubbing color fastnessLevel 4Friction for 20 cycles
Moisture resistant rubbing color fastnessLevel 4Friction for 20 cycles

Note:The product performance and application data listed above were obtained under specific experimental conditions,and the actual usage environment of the product is variable.Customers need to
undergo testing before mass production.For any unclear information,please contact Guangdong Caigle Technology Co.,Ltd.We reserve the right to revise the product manual without further notice.

5.Frequently Asked Questions

ProblemPossible CauseSolution
Paste Poor Crack1.Insufficient cross-linking time
2.The paste is not dry ,causing tearing due to peeling
1.Add additives in proportion
2.Operate according to the printing process
Poor Adhesion1.Insufficient cross-linking time
2.Insufficient overheating temperature and time
1. Let it stand for 8-12 hours
2.Overheating at 130-135℃ for 2minutes
Screen Plugging1.The paste is too thick
2.The humidity is too low
Add moisturizing agents with proportion not exceeding 3%