1. Product Description
1.1 Category:Special effects paste
1.2 Feature:Oxidation resistance,excellent fastness,soft hand feel,and non-sticky surface
1.3 Applicable fabrics:Suitable for all types of fabrics
1.4 Storage:Keep sealed and store in a cool and ventilated place between 5-40℃ of temperature
1.5 Eco-friendly:Compliant with OEKO-TEX and other relevant standards
2. ApplicationRatio

3. Printing Process
3.1 Printing condition
A. It is recommended to operate under 40% to 70%humidity conditions,and pay attention to the effect of temperature on operability.When the humiditshuy is higher than 70%,the
heating time shall be appropriately extended to avoid the surface becoming sticky and the washing fastness becoming poor;when the humidity is lower than 40%,1-3%moisturizer shall be added to
prevent the screen from blocking.
B. Squeegee:55-65 hardness oily squeegee
C. Mesh:80-100 mesh
D. Curing conditions:130-135℃ for 2 minutes
4.Performance Of Printed Products
| Test Project | 30F | Test Method |
| Flexibility | Level 4 | Internal standard:Level5 very soft |
| Elasticity | Level 3 | Internal standard:Level5 very soft |
| Machine wash fastness | Pass | 40℃Water temperature,20g of phosphate free laundry detergent,1000 rpm,standard wash for 90 minutes*5 times |
| Resistant to dry rubbing color fastness | Level 4 | Friction for 20 cycles |
| Moisture resistant rubbing color fastness | Level 4 | Friction for 20 cycles |
Note:The product performance and application data listed above were obtained under specific experimental conditions,and the actual usage environment of the product is variable.Customers need to
undergo testing before mass production.For any unclear information,please contact Guangdong Caigle Technology Co.,Ltd.We reserve the right to revise the product manual without further notice.
5.Frequently Asked Questions
| Problem | Possible Cause | Solution |
| Paste Poor Crack | 1.Insufficient cross-linking time 2.The paste is not dry ,causing tearing due to peeling | 1.Add additives in proportion 2.Operate according to the printing process |
| Poor Adhesion | 1.Insufficient cross-linking time 2.Insufficient overheating temperature and time | 1. Let it stand for 8-12 hours 2.Overheating at 130-135℃ for 2minutes |
| Screen Plugging | 1.The paste is too thick 2.The humidity is too low | Add moisturizing agents with proportion not exceeding 3% |