1. Product Description
1.1 Category:High temperature forming paste
1.2 Features:Application for manually printing and machine printing, resistant to collapse at high temperature
1.3 Applicable fabrics:Polyester fabric,nylon fabric,swimsuit fabric,etc
1.4 Storage:Keep sealed and store in a cool and ventilated place between 5-40℃ of temperature
1.5 Eco-friendly:Compliant with OEKO-TEX and other relevant standards
2. Application Ratio

3. Printing Process
3.1 Printing condition
A. It is recommended to operate under 40% to 70%humidity conditions,and pay attention to the effect of temperature on operability.When the humiditshuy is higher than 70%,the heating time shall be appropriately extended to avoid the surface becoming sticky and the washing fastness becoming poor;when the humidity is lower than 40%,1-3%moisturizer shall be added to prevent the screen from blocking.
B. Squeegee:55-65 hardness oily squeegee
C. Mesh:100-120 mesh
D. Curing conditions:150℃ for 2 minutes ,or 150℃ pressing 10-15 seconds
4.Performance Of Printed Products
| Test Project | 304H | Test Method |
| Flexibility | Level 3 | Internal standard:Level5 very soft |
| Machine wash fastness | Pass | 40℃Water temperature,20g of phosphate free laundry detergent,1000 rpm,standard wash for 90 minutes*5 times |
Note: The product performance and application data listed above were obtained under specific experimental conditions,and the actual usage environment of the product is variable.Customers need to undergo testing before mass production.For any unclear information,please contact Guangdong Caigel Technology Co.,Ltd.We reserve the right to revise the product manual without further notice.
5.Frequently Asked Questions
| Problem | Possible Cause | Solution |
| Poor foaming effect | The internal moisture was not completely dried, and the rapid evaporation of high-temperature moisture caused the surface to be uneven and granular | Dry at room temperature or bake at low temperature until dry |
| Insufficient overheating temperature and time | Overheating at 150℃ for 2 minutes | |
| Screen Plugging | The scraping is uneven and the surface is not smooth | Clean the screen plate and unclog the printed screen plate |