304H High-temperature Foaming Paste

Product Introduction

The foaming effect is excellent, and the surface is smooth and does not collapse after baking (the optimal fo aming temperature is 150-160℃*90S).


1. Product Description
1.1 Category:High temperature forming paste
1.2 Features:Application for manually printing and machine printing, resistant to collapse at high temperature
1.3 Applicable fabrics:Polyester fabric,nylon fabric,swimsuit fabric,etc
1.4 Storage:Keep sealed and store in a cool and ventilated place between 5-40℃ of temperature
1.5 Eco-friendly:Compliant with OEKO-TEX and other relevant standards

2. Application Ratio

3. Printing Process
3.1 Printing condition
A. It is recommended to operate under 40% to 70%humidity conditions,and pay attention to the effect of temperature on operability.When the humiditshuy is higher than 70%,the heating time shall be appropriately extended to avoid the surface becoming sticky and the washing fastness becoming poor;when the humidity is lower than 40%,1-3%moisturizer shall be added to prevent the screen from blocking.
B. Squeegee:55-65 hardness oily squeegee
C. Mesh:100-120 mesh
D. Curing conditions:150℃ for 2 minutes ,or 150℃ pressing 10-15 seconds

4.Performance Of Printed Products

Test Project304HTest Method
FlexibilityLevel 3Internal standard:Level5 very soft
Machine wash fastnessPass40℃Water temperature,20g of phosphate free laundry detergent,1000 rpm,standard wash for 90 minutes*5 times

Note: The product performance and application data listed above were obtained under specific experimental conditions,and the actual usage environment of the product is variable.Customers need to undergo testing before mass production.For any unclear information,please contact Guangdong Caigel Technology Co.,Ltd.We reserve the right to revise the product manual without further notice.

5.Frequently Asked Questions

ProblemPossible CauseSolution
Poor
foaming effect
The internal moisture was not completely dried, and the rapid evaporation of high-temperature moisture caused the surface to be uneven and granularDry at room temperature or bake at low temperature until dry
Insufficient overheating temperature and timeOverheating at 150℃ for 2 minutes
Screen PluggingThe scraping is uneven and the surface is not smoothClean the screen plate and unclog the printed screen plate